THOUSANDS OF YEARS OLD AND SOPHISTICATED

THE ART OF ENAMELLING

alangesoehne-emaille-ausgangsmaterial

The art of enameling has been around for about 3,500 years. Augustus the Strong, the Elector of Saxony, was a devotee of the technique. His court jeweler, Johann Melchior Dinglinger, created precious pieces in enamel, which are today on show in the Green Vault in Dresden’s Castle.

Enameling was also very frequently used to make the dials for pocket watches. These days, there are very few experts skilled in this highly complicated process, so that enameled dials are very rarely found in wristwatches.

THE ART OF ENAMELLING

The process of making an enameled dial takes several days, during which the different steps have to be repeated again and again. The greatest challenge: absolute cleanliness, to prevent the inclusion of the smallest particle of dust or dirt, which would mar the smoothness of the structure. “Enamel is capricious, and can’t be hurried,” Lange’s enamel experts explain.


alangesoehne-als-enamelling-2014-04-a4-16418

PREPARATION OF THE ENAMEL

First of all, the basic raw material, a special kind of glass, is reduced to microscopic fragments by rubbing and crushing in a mortar, so that it can then be sieved or applied wet with a brush.

alangesoehne-als-enamelling-2014_07_a4_16418

TREATMENT OF THE BACK

Counter-enamel is applied to the back of the dial. This is necessary to prevent distortion of the enamel on the dial side through excessive stresses.

alangesoehne-als-enamelling-2014-01-a4-15844

FILLING INTERSTICES

Small interstices between letters and figures are filled with enamel using a fine brush.

alangesoehne-als-enamelling-2014-09-a4-16418

SIEVING

The fine enamel powder is spread evenly over the dial with a sieve. The piece is then fired briefly at a temperature of several hundred degrees in a special kiln. These steps may be repeated several times.

alangesoehne-als-enamelling-2014-11-a4-16418

ENAMEL DUST

During sieving, the fine enamel dust is collected on a piece of aluminium foil.

alangesoehne-als-enamelling-2014-13-a4-16418

FIRING AND COOLING

After each firing, the dial is cooled slowly on a fireproof support. Only when the dial has been completely dried and cleaned can the sieving operation be repeated. This process takes several days.

alangesoehne-als-enamelling-2014-15-a4-16418

METAMORPHOSIS

The more enamel layers are applied, the darker the final surface appears. Thus, the blue shimmering enamel particles turn into the black dial eventually.